Copper-ColorAL process

Authentic copper shades ranging from pale pink to Bordeaux red

What is the Copper-ColorAL process? 

The Copper-ColorAL process is a two-step electrolytic dyeing process for achieving typical copper hues on anodised aluminium surfaces. The process is similar to the conventional colouring process used for tin and is carried out using the two-component product Alficolor 672 and Alficolor 692. 

Advantages:

Typical copper shades from pink to dark wine red on anodised aluminium

Electrolytically dyed oxide layers, thus high colour stability

Stabilised two-component system for uniform colouring and long bath life

Easily reproducible shades with simple maintenance effort

Colour variants possible by modifying c, t, T and acidity

Can be easily integrated into existing facilities

Plant equipment for colouring tin can be used

Individual components can be analysed


Simple mode of operation

Typical dyeing parameters:

15 g/l

25 g/l

20 g/l

Dyeing time


Temperature

Current

Alficolor 672

Alficolor 692

Sulphuric acid

0.5 – 15 minutes, depending on colour intensity

25 – 30 °C

AC, 50 Hz, 14-20 V, 0.2-1.0 A/dm²