<?xml version="1.0" encoding="UTF-8"?><rss version="2.0"
	xmlns:content="http://purl.org/rss/1.0/modules/content/"
	xmlns:wfw="http://wellformedweb.org/CommentAPI/"
	xmlns:dc="http://purl.org/dc/elements/1.1/"
	xmlns:atom="http://www.w3.org/2005/Atom"
	xmlns:sy="http://purl.org/rss/1.0/modules/syndication/"
	xmlns:slash="http://purl.org/rss/1.0/modules/slash/"
	>

<channel>
	<title>elektrolytisch Archives - Alufinish</title>
	<atom:link href="https://alufinish.de/en/tag/elektrolytisch-en/feed/" rel="self" type="application/rss+xml" />
	<link>https://alufinish.de/en/tag/elektrolytisch-en/</link>
	<description>Bauen auf Vertrauen - Build on trust</description>
	<lastBuildDate>Fri, 21 Apr 2023 10:34:51 +0000</lastBuildDate>
	<language>en-US</language>
	<sy:updatePeriod>
	hourly	</sy:updatePeriod>
	<sy:updateFrequency>
	1	</sy:updateFrequency>
	<generator>https://wordpress.org/?v=7.0.4</generator>

<image>
	<url>https://alufinish.de/wp-content/uploads/2018/01/cropped-logo512512.png</url>
	<title>elektrolytisch Archives - Alufinish</title>
	<link>https://alufinish.de/en/tag/elektrolytisch-en/</link>
	<width>32</width>
	<height>32</height>
</image> 
	<item>
		<title>The Tin ColorAL – colour variants</title>
		<link>https://alufinish.de/en/the-tin-coloral-colour-variants/</link>
		
		<dc:creator><![CDATA[Benedikt Wolter]]></dc:creator>
		<pubDate>Tue, 18 Apr 2023 16:56:04 +0000</pubDate>
				<category><![CDATA[latest news]]></category>
		<category><![CDATA[products]]></category>
		<category><![CDATA[Alficolor]]></category>
		<category><![CDATA[alufinish]]></category>
		<category><![CDATA[colouring]]></category>
		<category><![CDATA[elektrolytically]]></category>
		<category><![CDATA[elektrolytisch]]></category>
		<category><![CDATA[färben]]></category>
		<category><![CDATA[Zinn-Color]]></category>
		<guid isPermaLink="false">https://alufinish.de/?p=7728</guid>

					<description><![CDATA[<p>Electrolytical colouring with tin salts has been a popular process in anodising operations for decades. It can be used to produce numerous variants of bronze colourations (light to dark bronze), but also black surfaces on the aluminum base metal. While bronze shades were mostly predominant in recent decades, the process is now often used for [&#8230;]</p>
<p>The post <a href="https://alufinish.de/en/the-tin-coloral-colour-variants/">The Tin ColorAL – colour variants</a> appeared first on <a href="https://alufinish.de/en/">Alufinish</a>.</p>
]]></description>
		
		
		
			</item>
		<item>
		<title>Screen- and fried egg effect on electrolytically coloured aluminium</title>
		<link>https://alufinish.de/en/screen-and-fried-egg-effect-on-electrolytically-coloured-aluminium/</link>
		
		<dc:creator><![CDATA[Benedikt Wolter]]></dc:creator>
		<pubDate>Fri, 04 Nov 2022 19:32:13 +0000</pubDate>
				<category><![CDATA[error patterns]]></category>
		<category><![CDATA[aluminium]]></category>
		<category><![CDATA[electrolytically]]></category>
		<category><![CDATA[elektrolytisch]]></category>
		<category><![CDATA[error pattern]]></category>
		<category><![CDATA[färbung]]></category>
		<category><![CDATA[fried egg effect]]></category>
		<category><![CDATA[screen effect]]></category>
		<category><![CDATA[spiegeleieffekt]]></category>
		<guid isPermaLink="false">https://alufinish.de/?p=7299</guid>

					<description><![CDATA[<p>In classical, electrolytic colouring of aluminium surfaces with tin salts, uniform colourings from bronze to black are obtained with correct operation and the right colouring bath settings. However, sometimes you can observe inhomogeneous colouring on the goods carrier, so that a glance at the goods is enough to recognise the non-uniformity. Typical electrolytic colouring process [&#8230;]</p>
<p>The post <a href="https://alufinish.de/en/screen-and-fried-egg-effect-on-electrolytically-coloured-aluminium/">Screen- and fried egg effect on &lt;strong&gt;electrolytically coloured aluminium&lt;/strong&gt;</a> appeared first on <a href="https://alufinish.de/en/">Alufinish</a>.</p>